Hi, after the first not successful mold and part (http://www.talkcomposites.com/Topic36543.aspx) I worked on the part to fix the issues in order to build a new mold.
This time the part popped from the mold almost by itself but... something has happened to the tooling gelcoat!
Please se pics. Last pic is the tooling gelcoat on the base glass, so I tend to exclude some interaction with the plug.
Any ideas?


Attachments
20200814_151808.jpg (365 views, 1.00 MB)
20200814_152504.jpg (340 views, 2.00 MB)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
mporta71 - 6 Years Ago
Warren (Staff) - 6 Years Ago
mporta71 - 6 Years Ago
Warren (Staff) - 6 Years Ago
mporta71 - 6 Years Ago
mporta71 - 6 Years Ago
beliblisk - 6 Years Ago
mporta71 - 6 Years Ago
beliblisk - 6 Years Ago
mporta71 - 6 Years Ago
beliblisk - 6 Years Ago
                                         Definitely yes! Thank you!
mporta71 - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search