Hi everyone,

I’m not new to skinning parts as I have done a lot on my car but they haven’t been overly complicated in terms of intricacy, however I have found like most when I have done some intricate parts with varying contours and so it is hard to get the carbon to stick.

Be it glue or resin I use to adhere the carbon what would I need to go down the bagging route for intricate parts?

Is it a case of the usual prep, apply adhesive then carbon, into a bag and remove air? Or do I need anything else?

Thanks
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Stucross - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search