Hi, just a quick question. I'm making a few house number plaques at the moment. I've power carved the numbers out and filled with your 10/50 resin. I mixed 100ml of resin to 50ml of hardener and added ten drops of black dye.
My question is would this amount of dye in such a small amount of resin retard the curing time.