Using 3D printed part for a core to overcoat with epoxy and carbon / hand layup


Using 3D printed part for a core to overcoat with epoxy and carbon / hand layup
Author
Message
Joe LaCour
J
Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)
Group: Forum Members
Posts: 4, Visits: 15
I have an idea to make a component out of carbon fiber and in the past i would have carved up some foam for a core and overlaid epoxy and glass or carbon fiber.

Now that I have a 3D printer, I am considering printing the core and overlay with cloth and epoxy.

When searching the forum, I found only references to using 3D printing for a mold.  Maybe I did not search correctly.  Has there been anyone with experience doing this?  The core would be in several pieces and bonded together.  Preferably PLA and West System epoxy.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Joe LaCour - 6 Years Ago
LibertyMKiii - 6 Years Ago
LibertyMKiii - 6 Years Ago
Joe LaCour - 6 Years Ago
Joe LaCour - 6 Years Ago
LibertyMKiii - 6 Years Ago
     Thanks
Joe LaCour - 6 Years Ago
CeeBee - 6 Years Ago
janherich - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search