Should I have made mould deeper?


Author
Message
carbon man
carbon man
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Awaiting Activation
Posts: 86, Visits: 1.2K
I have moulded this fuel cover but struggling to make the part without bridging around the edge. This is prepreg.

I'm laying 1 xpreg surface ply and 1 backing ply. Laying it in one full piece. And tried debulk for 30mins to.

Should I have made the mould of filleting wax a bit deeper? Or should I be laying a circle of carbon and then go around the edge. But as this is a cover I figured I couldn't do that and overlap the carbon joins making it to thick. 

Thanks


GO