Hi RRE,
By the looks of that part I would say that no mould would be needed, you could do that from flat sheet and trim to final shape and drill the holes... This method would also give you the ability to make a double "a" sided part by simply bonding 2 half thickness flat sheets back to back to give you the final thickness you require... Also not to mention that you could use the original as a "jig" to trim with a router and the holes as a way to mount the jig to the part while you route it out...