I recently used your carbon fibre skinning kit on a car product. I measured the resin to exactly 3:1 ratio in good conditions at the start of summer. 
The resin cured fine and I got it to a great finish. 

However 4 days after installing the product in the outside of the car the direct sunlight has caused the resin to form ripples in line with the carbon fibre. They are all equal straight lines. The resin has developed a greyish tone to it.

Can you explain why this has happened. I am working on two other car parts and I'm afraid to out them on the car in case the same thing happens.

Thanks
B
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
BMac - 6 Years Ago
SleepingAwake - 6 Years Ago
BMac - 6 Years Ago
BMac - 6 Years Ago
Hanaldo - 6 Years Ago
MarkMK - 6 Years Ago
BMac - 6 Years Ago
SleepingAwake - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search