I have a barrel lid from a whiskey barrel and the back of it is all burnt which i want to stabilise and end up with a nice clear resin coating.

Not too bothered by how much of a coating i end up with but the thicker the better

The problems i foresee is mainly that there is quite a lot of loose carbon which i would like to keep in place


So how would you go about this and what materials would you use