Hello,

I am carbon fiber wrapping a slice of an RC plane wing for testing using vacuum bagging. After the layup, the easy release fabric and the breather material are both epoxy hardened and STUCK to the part. I recognize this part is scrapped, but what would you estimate the problem to be? It doesn't feel like too much epoxy, but what else could it be if it's soaking through and hardening everything. Should I try and really squeeze epoxy out before vacuum bagging? Or are the easy release and breather fabric just trash? Any suggestions would be greatly appreciated.

Thanks,

Simeon

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search