Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Clear cast resin
Clear cast resin
Post Reply
Like
2
Clear cast resin
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Anthony kennedy
A
Anthony kennedy
posted 5 Years Ago
ANSWER
HOT
Topic Details
A
Group: Forum Members
Posts: 2,
Visits: 9
I need to know how much resin I need for my project as I can not work this out the size is 106 inches long 20 inches width and 10 millimetres deep could some one please help and let me know how much I need
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Clear cast resin
Anthony kennedy
-
5 Years Ago
Length x width x depth x density (106×0.0254)×(20×0.0254)×0.01×1200 ~ 16.5kg This is with no margin, so you probably want a good bit more and maybe double check the density in the tds, but 1200kg/m3....
SleepingAwake
-
5 Years Ago
Thanks very much
Anthony kennedy
-
5 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search