Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Is my lip ready for clear coat?
Is my lip ready for clear coat?
Post Reply
Like
4
Is my lip ready for clear coat?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
TheMidnightNarwhal
T
TheMidnightNarwhal
posted 5 Years Ago
ANSWER
HOT
Topic Details
T
Group: Forum Members
Posts: 10,
Visits: 51
I sanded my last coat of epoxy and ready to apply clear coat. I did 180 grit on most of it but in spots that had a lot of resin to level out I used 80 griot then passed over with 180 after.
Now I did a final 600 grit wetsand in preparation for clear coat but as you can see in pic some areas seems to still show some 80 grit marks? I went over few times but it won't remove those. Is that fine? Can I proceed with clear coat?
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Is my lip ready for clear coat?
TheMidnightNarwhal
-
5 Years Ago
No, you will see those scratches very easily. Worst bit is they may actually look acceptable as soon as you spray it, but over time the clear will sink back into those scratches and it will look wors...
Hanaldo
-
5 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search