	Group: Forum Members 	        
    Posts: 2.5K, 
    Visits: 28K 
    
 
          
		     | 
				                       
                 
                
                    
			            For a big plug, I would use a conventional HVLP spray gun, or a Preval sprayer if you dont have the equipment to spray. You will waste a lot in overspray but the results are significantly better. Wear a respirator though!
                  
			            				
			                                 
                     
                                            
                         
                    
                  
             |