I'm trying to seal a large plug before making the mould as it's not hugely strong and I want to be certain it will release. When I use the EC provided spray nozzle for the S120 it gives patchy coverage and creates high and low spots. The nozzle isn't a very uniform spray. What's the best way to apply this to a big plug, does the long free cloth method work as well? Would welcome any experiences as its taken me weeks to sand off the sprayed S120 back to a smooth finish. Thanks
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
For a big plug, I would use a conventional HVLP spray gun, or a Preval sprayer if you dont have the equipment to spray. You will waste a lot in overspray but the results are significantly better. Wear a respirator though!