Noob question, sorry but there's no clear answer that I could find. 
I'm seeking a rod that is flexible enough to be wound up but which would prefer to be a straight line.
Imagine one of those auto-erecting tents that fold up into a round bag, but in this case would fold up to around 15cm diameter. Something like that would serve that purpose when piped into the outline of fabric.

I think 1, 2, or 3mm carbon rod may do for what I need but I'm not sure.

Thanks.
Edited 6 Years Ago by nigelws
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
At the bottom end of the scale, the 1mm rods will coil easily enough, we have had to do that to send one by post where the cheapest possible shipping was requested by the customer.

The bigger diameter rods can be coiled up to around 4mm but the diameter is much bigger and you would probably need to experiment to find the right kind of curvature without it breaking.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
nigelws
n
Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)
Group: Forum Members
Posts: 3, Visits: 7
Ah, shipping is a good example. Could you coil a 2mm or 3mm diameter 2000mm rod into a padded C4 (A4) envelope?
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
1mm will coil easily, the others probably wouldn't coil enough to ship in that size and such would go in a tube.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
nigelws
n
Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)
Group: Forum Members
Posts: 3, Visits: 7
Thanks. That's really helpful. Is the 1mm rod likely to kink at all?