When you make the pattern, you will need to block the vents, mould off it thus giving a mould with no vent holes in it.
You create the vent holes when you lay up the fabric. In simple terms you do not lay fabric over the vent hole areas except around the very edge so you have something to trim. You want a small bit to trim as no matter how neat you are, the carbon raw edge is always a bit rough.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|