Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Best way to do most 2-piece carbon joins is with a stepped lap joint. This is pretty easy to do with wax sheet, but it does add a couple of steps to your mould making process.
That said, I don't feel like that is necessary for something as simple as an AirPods case, unless you have a weird complex design rather than the usual design? In any case, a simple 2 piece mould that gets laid up separately before bolting the mould together and curing as one piece would be the best and easiest way for me.
|