Best way to make moulds from FDM printed ASA prototypes.


Author
Message
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
To use a tooling pre-preg to make your moulds, such as our XPREG XT135Tooling Prepreg,  then your plastic needs to be able to go to 60C as a pattern for the mould.  The rest of the pre-preg cure is done with the pattern removed. So the ASA seems fine on temperature.

In terms of wet lay up, a pre-preg mould will be suitable to make wet lay up parts as well as pre-preg parts so you would not need 2 different moulds. 

Ensure you use a release agent which can handle the 60C such as our Easy-Lease Chemical Release Agent



Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
DonV
D
Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)Junior Member (18 reputation)
Group: Forum Members
Posts: 1, Visits: 9
I am getting (delivered tomorrow) 3 FDM printed ASA plastic prototype aerofoils, maximum dimension 600 mm.
I hope to use these
1.    for quite a few months of functional testing,
2.    for making a mould from which to produce lightweight carbon-fibre replicates of the prototypes.
Perhaps you can advise me what surface treatment would suit these aims.
I want a high-gloss finish that
1.    Will not compromise the ASA plastic parts. A compatible system that will not weaken the parts or cause surface cracking.
2.    Suits making moulds using wet lay-up.
3.    Suits making moulds using pre-preg. carbon fibre. In this case the ASA plastic parts must not be heated beyond ASA softening temperature (>90C).
What processing and materials would you advise?