Dezer
Dezer
posted 6 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 74,
Visits: 1.8K
Carbon fiber parts over 15 years old with a
yellowish appearance.
- How to make it look new again?
- Sanding the entire surface and applying a new clearcoat will solve?
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Restoring old carbon fiber parts (yellowish).
Dezer
-
6 Years Ago
No,the "yellowing " is ageing through the resin not just on the surface
f1rob
-
6 Years Ago
It can be possible, it depends how bad it is. You have to remove all of the yellowed resin, so sometimes this can mean you hit fibres before you get rid of it and in this case theres nothing you can....
Hanaldo
-
6 Years Ago
I am going to risk this sanding technique to remove as much of the varnish and yellowish resin layer as possible. I'm going to risk the method of pigmenting the clearcoat with black, the part will...
Dezer
-
6 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search