+x Miles Beharrell - 4/12/2020 10:56:02 AMHI AllI have just completed by first carbon wrap using a starter kit. Its a c/f tube for carrying fishing rods. I have wet laid it and although its pretty rough and ready its as you would expect for a first attempt. I wrapped the c/f around a plastic tube which I coated with PVA release agent from EC. Just no way this is coming off though! Any tricks or hacks would be really appreciated to (1) get the c/f tube off (2) better ways to do next time. Thanks allM
+x KM Composites - 4/12/2020 1:41:01 PM+x Miles Beharrell - 4/12/2020 10:56:02 AMHI AllI have just completed by first carbon wrap using a starter kit. Its a c/f tube for carrying fishing rods. I have wet laid it and although its pretty rough and ready its as you would expect for a first attempt. I wrapped the c/f around a plastic tube which I coated with PVA release agent from EC. Just no way this is coming off though! Any tricks or hacks would be really appreciated to (1) get the c/f tube off (2) better ways to do next time. Thanks allMI found Easycomposite video very helpful for making carbon fibre rods https://www.easycomposites.co.uk/vacuum-bagging-sealant-tape/how-to-make-a-roll-wrapped-carbon-fibre-tube