Bonding carbon fibre to uPVC


Author
Message
David Bligh
D
Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)Junior Member (8 reputation)
Group: Forum Members
Posts: 1, Visits: 1
Hi,
I need to electrically insulate a carbon fibre tube used to support an electrode.  Is it possible to bond upvc to carbon fibre to give an insulated "sandwich" whilst maintaining a structural support as well as electrical isolation? 