Group: Forum Members
Posts: 1,
Visits: 4
|
Hello ,
I have a box of 10x translucent pigments, easycomposites, will they still work with the glasscast 3/10/50? I bought some glasscast a few years ago and do get air bubbles sometimes, I do small projects and only have a basic set up, can you tell me which if any of the clear epoxies 3/10/50 is more or less susceptible to air retention? I get good results mostly butt its been a while since I last bought and curious to know things have changed. Thanks for your time, Liam.
|