Hello,

I first used the VM100 Black 10min Methacrylate Adhesive one year ago. I tested again one week ago to glue one piece of nylon with an aluminium part without any flame treatment. The result was good. I had to apply a huge force by hand to dissassemble both parts (40 mm^2 glue surface).

On your website page of the product, you describe the life expectancy of the product of 12 month on the shelf. Do you mean that the shear strength will reduce a little bit after 12 months or ist here a huge reduction of the shear strength of the bonding ? In my application, I'm expecting the max shear stress of 0,05 MPa (N/mm^2) which does not seem to be a huge stress. 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search