liamogoliver
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 5
Hey,
New to carbon fibre, attempting to make a female mould using MDF, need internal fillets on the mould in the attached image, any recommendations on filler material would be greatly appreciated, the fillets need to be 40mm radius, also any recommendations regards a sealer type/brand that I should use. Looking to make some male moulds with MDF so any info regards using MDF as a mould material would be great!
Cheers.
Attachments
27112012251.jpg
(
428 views,
840.00 KB
)
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
MDF Mould for Formula Student Nosecone
liamogoliver
-
13 Years Ago
Its a little confusing by the words you are using. If you are making a nosecone plug out of MDF that...
fgayford
-
13 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search