Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Projects
»
Motorsport, Vehicle Design and Modification
»
Carbon fiber air intake
Carbon fiber air intake
Post Reply
Like
8
Carbon fiber air intake
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
DustinPeters
DustinPeters
posted 14 Years Ago
ANSWER
HOT
Topic Details
Group: Awaiting Activation
Posts: 2,
Visits: 17
Hey, I'm trying to figure out the best way to make a carbon fiber air intake for a car using braided carbon fiber sleeve. I need to know what the best type of resin would be for it, it needs to be both durable and have a nice finish. It doesn't need to be extreme hear resistant.
Thanks,
Dustin
Reply
Like
8
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Carbon fiber air intake
DustinPeters
-
14 Years Ago
Hi Dustin, I guess the resin choice depends on how you plan to make this intake. Assuming you'll...
Matt (Staff)
-
14 Years Ago
Hey Matt, thanks for all the information that is very helpful. The plan is to wet laminate the part...
DustinPeters
-
14 Years Ago
Hi Dustin, You're welcome. For general advice and ideas on this it might be worth chatting it...
Matt (Staff)
-
14 Years Ago
Ive moved this over so it gets better coverage by the usual members.
Warren
-
14 Years Ago
I have looked into doing this before, the best idea I came up with was to make 2 moulds, to make the...
Sharper
-
14 Years Ago
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search