Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Projects
»
Motorsport, Vehicle Design and Modification
»
Prototype Rear Wing MK 2 The Evolution
Prototype Rear Wing MK 2 The Evolution
Post Reply
Like
3
Prototype Rear Wing MK 2 The Evolution
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
wozza
wozza
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
Cheers. Some more pics in photobucket carboncopiesltd.
Carbon
Copies Ltd
Edited
12 Years Ago by
wozza
Reply
Like
3
brasco
brasco
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 192,
Visits: 305
sweet!
CarbonFiberCreations
Reply
Like
3
wozza
wozza
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
There you go
Carbon
Copies Ltd
Reply
Like
3
brasco
brasco
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 192,
Visits: 305
if no pics then it never happened. oh by the way, where are the pics ???
wozza (24/11/2012)
Finally finished the MK 2 version of the Wing.
As with the first one the angle of attack can be adjusted via the turnbuckles but in addition the end sections can be adjusted separately to the main wing.
Regards Warren
CarbonFiberCreations
Reply
Like
3
ajb100
ajb100
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 346,
Visits: 4.4K
Chris posted these pics on Facebook the other day, looks good!
Reply
Like
3
wozza
wozza
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
Managed to get the wing fitted to the car ready for some winter testing.
Carbon
Copies Ltd
Reply
Like
2
Matthieu Libeert
Matthieu Libeert
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
good work, nice and clean
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
wozza
wozza
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
Finally finished the MK 2 version of the Wing.
As with the first one the angle of attack can be adjusted via the turnbuckles but in addition the end sections can be adjusted separately to the main wing.
Regards Warren
Carbon
Copies Ltd
Edited
13 Years Ago by
wozza
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search