Mould in XPS


Author
Message
Massimiliano
M
Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)Supreme Being (2.4K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Hi, I know polyurethane foam is better but is not easy to find and costs a lot for large molds, so I would like to use polystyrene foam or XPS.
When I am done with shaping the plug, what could I use to cover it to sand flat and smooth until a polished state?