Do I need more layers of fibreglass?


Author
Message
Classicarbon
C
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 86, Visits: 639
Made mould,dry nicely but still can see through gelcoat.I mean it not went completely " milky". I used 3 layers.One for coupling coat and 2 after.
Should I apply another layer of fiberglass?
picture was taken  before full cure.