Hi there,

Is there a reason NOT to use a perforated heat shrink tape when doing a wet layup around a cylindrical object to get rid of the excess resin?

As I can't see it on the Easycomposite website, can I use standard tape and make holes with a pin? Or will the tension tear the tape off the part once heat is applied?

Many thanks,
P.

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Physicx - 6 Years Ago
Warren (Staff) - 6 Years Ago
Physicx - 6 Years Ago
SleepingAwake - 6 Years Ago
Fasta - 6 Years Ago
Fasta - 6 Years Ago
Physicx - 6 Years Ago
oekmont - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search