Glad to hear the project went well for you.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
oneohtwo
o
Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)
Group: Forum Members
Posts: 15, Visits: 220
Warren (Staff) - 2/12/2020 10:37:30 AM
If you give the gelcoat a good key with 120 grit paper and thorough clean  you should be fine.  A wipe over to clean with acetone might even help make the surface a little tacky again. 

This worked fine, thanks. I wasn't able to get back to it for a week, and the gelcoat still had a bit of 'grab' when I came to give it a key. It (mostly) all removed from the plug fine. 

Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
If you give the gelcoat a good key with 120 grit paper and thorough clean  you should be fine.  A wipe over to clean with acetone might even help make the surface a little tacky again. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
oneohtwo
o
Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)Supreme Being (257 reputation)
Group: Forum Members
Posts: 15, Visits: 220
I wanted to check if it is still ok to lay down a coupling coat on top of a gel coat that has fully cured? Due to some unforeseen circumstances outside my control I was interrupted at the weekend when laying up a mould using the uni-mould system. Unfortunately I was only able to put down the gel coat. This will therefore have had 48 hours+ (probably most likely 56)  of curing before I can put down the coupling coat.

The gelcoat had a catalyst at about 2%, and has been curing in temp range between about 20-27 degrees. It has hardened and as of this morning had no discernable 'tackiness'. I just want to check it is still viable to lay down the coupling coat and 150csm? I imagine there should still be a bond between the two, but would it be advisable to put a key in the gelcoat?

Additionally i won't be able to finish off with the 450csm and tooling resin until the weekend, but I see previous advice on this forum suggests that will be fine if I key the coupling coat.

Many thanks.


Edited 6 Years Ago by oneohtwo