idcomp
i
idcomp
posted 6 Years Ago
ANSWER
HOT
Topic Details
i
Group: Forum Members
Posts: 5,
Visits: 55
Hi all,
Having problems with resin being too runny. I put two coats then light sand with 240grit then one more coat. And still resin is too thin on some places like curves it just runs off even if I put thicker coat.
I mix resin and hardener and wait for about 5-10 min for it to degas
Had this problem before. You can see it in the pic where on such a little slope it just wont stay in place just runs off.
How to deal with this problem?
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Skinning resin viscosity
idcomp
-
6 Years Ago
Generally speaking, the XCR coating resin is quite thick and on the first couple of coats, excessive running shouldn't be too much of an issue on vertical sides, given that you'll be giving it quite ...
MarkMK
-
6 Years Ago
I didn't mention I don't use XCR resin. I use this one https://shop1.r-g.de/en/art/100110
idcomp
-
6 Years Ago
The resin is advertised as a low viscosity resin. Might be worth looking up the TDS to check and compare. A low viscosity resin may well be the cause of your issues. For example, the XCR coating...
Warren (Staff)
-
6 Years Ago
What am I looking for exactly? Left resin mixed for about 35-40mins at about 20c its thicker but not sure will it help. Will see and report back. Also is it good idea to spray acetone to get rid of...
idcomp
-
6 Years Ago
Look for the Viscosity properties in centipoise. Laminating resins tend to have a viscosity of around 350-600cps. Coating resins like the XCR resin are normally thicker, around 800-1000cps. No, or a...
Hanaldo
-
6 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search