Tom (Staff) - 12/13/2019 9:13:03 AM
David Blackmore - 12/13/2019 8:50:48 AM
Can anyone tell me how much metallic pigment by weight I would need to colour 12kg of Glass Cast 3 please?.

Hi David, An easy way of working this out would be to know that 20g of metallic pigment will cover 3kg of resin. So 80g would be plenty to cover the 12kg of resin you have. 

Thanks Tom

Tom (Staff)
T
Supreme Being (281 reputation)Supreme Being (281 reputation)Supreme Being (281 reputation)Supreme Being (281 reputation)Supreme Being (281 reputation)Supreme Being (281 reputation)Supreme Being (281 reputation)Supreme Being (281 reputation)Supreme Being (281 reputation)
Group: Moderators
Posts: 21, Visits: 977
David Blackmore - 12/13/2019 8:50:48 AM
Can anyone tell me how much metallic pigment by weight I would need to colour 12kg of Glass Cast 3 please?.

Hi David, An easy way of working this out would be to know that 20g of metallic pigment will cover 3kg of resin. So 80g would be plenty to cover the 12kg of resin you have. 

David Blackmore
David Blackmore
Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)
Group: Forum Members
Posts: 2, Visits: 2
Can anyone tell me how much metallic pigment by weight I would need to colour 12kg of Glass Cast 3 please?.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search