Harsh, but I kind of agree with Robs point ^
Releasing a mould isn't hard, it just takes some care. Do things methodically to ensure you get full coverage, and just pay attention while you're doing it, don't be distracted by something else. I've never come across a mould that's so complex that you can't get full release coverage.
With that in mind as well, are you sure your sticks are actually due to incomplete coverage? Perhaps there is another issue going on there.
|