			            I am about to make a plug from 25mm closed cell PVC profiles. I chose this rather than a skeleton filled in with low density as in the video. I don't want to use hot melt glue to hold them together. I'd like a bit more time to align and I want to get the profiles flat to each other.. What glue should I use? I know to keep it away from the edges. Would PVA be good?  Thanks - Jonathan Woolrich                   
			            				
			                                 
                     
                                            
                         
                    
                  
             |