Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
If the parts already have no overlap on the edges, then bond on the joint to hold in place, then laminate carbon tape or cut strips of carbon fabric in several layers over both sides of the join to give actual strength.
If they are still in the design stage then I would engineer an overlap, probably on the bottom for ease, to ensure you have a good large bonding area to bond the 2 parts together.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|