Hi Steve,
Sorry for the delay in getting back to you about this point, I know we've developed a new method for you now which is working a treat so this is somewhat a mute point but to help others out there, it's oftena good idea to combine a pressure bag with a vacuum bag. The vacuum will help to get any trapped air out of the laminate whilst the pressure bag puts the real pressure on. This would probably help with the pin holes quite a bit.
Best regards, Matt