Hi, I'm completely new to epoxy resins but was looking to experiment with a smaller piece of timber before I tried something larger. SO I ordered a piece of waney edged timber on ebay, but the thickness was only 18mm. Will GlassCast 50 work here? Looking at the river table video, I was going to seal the under side, pour the river but then also use the same to do a top flood. Would this work?