vacuum bagging


Author
Message
smp4616
s
Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)
Group: Forum Members
Posts: 5, Visits: 37
Hi, has anyone achieved a void and pinhole free surface on carbon fiber using the wet layup and vacuum bagging technique?  I've been using infusion for years since I last gave up on bagging, but I feel like if I could get the surface I'm after with bagging, it would help with production on some more common parts.  
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search