Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Mould Making
»
Fiber flass resin mix?
Fiber flass resin mix?
Post Reply
Like
2
Fiber flass resin mix?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Classicarbon
C
Classicarbon
posted 6 Years Ago
ANSWER
HOT
Topic Details
C
Group: Forum Members
Posts: 86,
Visits: 639
Start having problem with resin after mix with MEKP. I was mixing 1.5% ratio and resin very quick become gelly,about after 10min.
Might be to warm in the garage?
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Fiber flass resin mix?
Classicarbon
-
6 Years Ago
Yes, resin will tend to 'go off' much quicker than gel coats and temperatures above 20 degrees will accelerate things quite a lot Be wary that some catalysts will be formulated to be fast acting als...
MarkMK
-
6 Years Ago
Can't put less catalyst? That won't slow things down?
Classicarbon
-
6 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search