Sounds like you are right on the limit of what the rod can bend to. Can you use a smaller diameter rod? or is the strength insufficient?
If you could find a tube of the right overall diameter, you could hand lay up carbon fibre to make pre-bent rings. They would not be as neat as a pultruded rod, but with care you could make a neat and fairly consistent carbon band. I would probably look at using carbon tow to help improve the hoop strength.