Group: Forum Members
Posts: 3,
Visits: 93
|
Hello , im doing a spoiler prototype , i want to make a mould of this spoiler in fiberglass I want mould resists a lot of copys , i thinked the best way os gel coat epoxy grey high temperatures for prepegs, fiber glass , and epoxy resin . The copy will be do with top coat poliester , fiberglass and poliester resin. It is compatibility? Thanks , sorry for my english
|