Air/resin bubble issues.


Author
Message
David Bond
D
Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)
Group: Forum Members
Posts: 2, Visits: 12
Howdy,
I am working with a group of US veterans teaching them composite prepreg layup techniques and am having problems with what are either air bubbles or resin bubbles. Here is a pic. under a 10x300x microscope:
Any suggestions as to what is wrong?