Hi all,

I want to make some covers for bike parts that they could fit over the existing part as a cover. But what is the best way to do this?
I need to somehow make the mould bigger then the original part i take the mould from. Any one can tell me how to do this?

Thanks

Thom
Rich (Staff)
Rich (Staff)
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Administrators
Posts: 167, Visits: 4.6K
Sheet Wax is used to offset the surface of the part, it is wrapped over the piece and then the mould is taken directly off the surface of the Sheet Wax, thus the mould tool ends up slightly bigger than the original part. When you then make the part, it too ends up slightly bigger than the original. We have it available in 1mm, 2mm and 5mm sheet thicknesses; you can find it by following the link: https://www.easycomposites.co.uk/232g-plain-weave-carbon-fibre-tape/Mould-Making-Materials/sheetwax.html
Thomb
Thomb
Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)
Group: Forum Members
Posts: 23, Visits: 656
Thanks! didnt even know u had these!!
Rich (Staff)
Rich (Staff)
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Administrators
Posts: 167, Visits: 4.6K
No problem Thomb Smile
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search