Hi all,

I am new to composites and I am currently trying to skin some parts for my car.

To begin, I had issues with bonding the fabric to the parts but I have seemed to solved my issue by not folding the excess behind the part for a clean edge. My main issue at the moment is sanding. I am struggling to get a nice flat surface and I am reluctant to use 120 to begin flatting as I always end up with scratches I struggle to sand out. What is the most efficient way to get a smooth finish without sanding forever. Also, what is the best way to remove drips that have cured and also a bulging edge where the resin has collected on a vertical edge on a part? I worry when I’m sanding I will hit the fabric.

My last issue seemed to be on the weave when I finished sanding, it looks like a void between the resin and the weave as well as moisture under the resin when damp outside.

I am using XCR resin and have been told it is self levelling and does not have air bubbles but I keep getting bubbles!

Thank you


Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Also watch the temperature you are working at.  Much above 20C and the XCR viscosity drops a fair bit and that can cause issues with fisheying and getting uneven coats etc.  

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
LukeSGee - 6 Years Ago
MarkMK - 6 Years Ago
Warren (Staff) - 6 Years Ago
LukeSGee - 6 Years Ago
MarkMK - 6 Years Ago
Warren (Staff) - 6 Years Ago
LukeSGee - 6 Years Ago
Warren (Staff) - 6 Years Ago
MarkMK - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search