Is it possible to make resin carbon fiber composite having a hard surface?


Is it possible to make resin carbon fiber composite having a hard surface?
Author
Message
westcomposite
w
Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)
Group: Forum Members
Posts: 11, Visits: 43
Thanks
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
I am not aware of any "toughened" coatings you can apply to the resin to make the surface tougher or harder.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
westcomposite
w
Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)
Group: Forum Members
Posts: 11, Visits: 43
I know the resin+Carbon fiber combination usually make a soft surface, with friction, the surface is easy to be damaged.
However, if I spray some coating on it after finish, can the things be changed? Is there any coating like that?