Hi.
If you have an undamaged one, you can use that to take a clean mould. You need to carefully inspect the damaged one to try and work out the lay up and materials used in its construction. You may well find several different cloths and/or layups depending where on the blade it is.
Ideally take some advice from someone who has made these kind of blades before.
The project could well cause you or others serious harm if you get it wrong as blade fragments from a disintegrating blade make nasty shrapnel, so take extra care.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|