mdoru
m
mdoru
posted 7 Years Ago
ANSWER
HOT
Topic Details
m
Group: Awaiting Activation
Posts: 7,
Visits: 162
Hello there guys !
I am doing some skinning works with CF and until now I've been using a 2 part black by color brushable adhesive and everything was amazing but now they discontinued the product, so I found myself in a situation. Can someone help me with some alternatives to obtain a perfect bond before using the resin with the parts ?
Some of the parts have shapes(see attached picture) and I really don't want to find myself in a awkward situation finding them with the fabric apart the part at corners the next day. I did a little research but I have found nothing similar to this product I've been using.
Any suggestion is appreciated.
Thank you !
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Bonding adhesive
mdoru
-
7 Years Ago
Is it not similar to Easy Composites black XCR epoxy?
Hanaldo
-
7 Years Ago
To be honest I don’t really know. I have just checked the XCR description. The one I’ve been using was really sticky when brushed and ussualy it takes 5 6 minutes (20 celsius) per layer to dry out,.....
mdoru
-
7 Years Ago
No, not by the sounds of it. But it will achieve the same objective of tacking the fabric into place, you will just have to get used to different application techniques. Watch the Easy Composites XC...
Hanaldo
-
7 Years Ago
In essence you were using an adhesive where as the XCR Black Epoxy Basecoat is very much a liquid resin. It takes approximately 2 hours to reach the firm but tacky stage, at which point you can apply...
Warren (Staff)
-
7 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search