HI,
You would certainly want to remove the cup holder and storage area flaps as a separate project. Perhaps if the lighter storage box can actually be removed, that would simplify things a lot.
Clips on the back are normally done afterwards and bonded into place. You may need a bit of redesign of how you fix it to the car.
Other than that, you need to block all the holes and then its relatively conventional moulding process. Just double check the sides don't mean the part would mechanically lock into a one part mould. If it looks like it will, you may need to go to a 2 piece mould or more.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|