ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
What are you trying to pigment? The silicone mould or the resin part? Which silicone pigment is it?
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
4
flooddylan
flooddylan
posted 7 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 9,
Visits: 51
Can you remind me how much silicone pigment I add to get strong colour without affecting the mix negatively?
Many thanks!!
Floodylan
Reply
Like
5
Andyconcorde
A
Andyconcorde
posted 7 Years Ago
ANSWER
HOT
Post Details
A
Group: Forum Members
Posts: 2,
Visits: 40
Excellent thank you
Reply
Like
4
Rich (Staff)
Rich (Staff)
posted 7 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 167,
Visits: 4.6K
To put it in straight-forwards terms; for every 100g of Silicone, you need to mix in 5g of catalyst
As examples:
20g silicone = 1g catalyst
300g silicone = 15g catalyst
500g silicone = 25g catalyst
Reply
Like
4
Warren (Staff)
Warren (Staff)
posted 7 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
PBW is "Parts by weight" so you can measure it by weight in grammes or kilos no problem just using the 100:5 ratio.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
5
Andyconcorde
A
Andyconcorde
posted 7 Years Ago
ANSWER
HOT
Topic Details
A
Group: Forum Members
Posts: 2,
Visits: 40
Hi
I am new to this so please bear with me.
With the silicone cs25 the recommended ratio is 100pbw silicone to 5pbw to catalyst, what does this relate to in Grammes or kg please
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search