Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Yeh as above, just do a local repair, there's no need to remove the surrounding gelcoat. Just mask off a square around the damaged section (so you don't sand the surrounding area), and then feather out the damaged gelcoat with 120 grit sandpaper until it is nearly flat with the exposed carbon. Apply some clear coat, let cure, flat down with 800 then 1200, then polish. Less than an hours work in it.
|