Nupur Dasgupta
Nupur Dasgupta
posted 7 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 4,
Visits: 17
Hi,
I made a river table with glass cast 50. I sanded and polished it already, but I am thinking to pour one final top coat, can I use glass cast 3 for this pourpose?
Thanks
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Using glass cast 3 as a final coat on river table.
Nupur das gupta
-
7 Years Ago
Good Morning, yes of course, GlassCast 3 is ideal to use for a top coat as it cures with a perfectly smooth glossy finish. To make sure that the GlassCast 3 bonds to the 50, you will need to give the...
Tom (Staff)
-
7 Years Ago
Thank you so much.
Nupur das gupta
-
7 Years Ago
I poured glasscast 3 as top coat, I am very happy with the clear gloss effect. But unfortunately there are some dust particle, they are quite visible. Can I sand it to remove those dust particle and....
Nupur das gupta
-
7 Years Ago
Good Morning, Thank you for getting back to me. You can use some abrasive paper going up in grits. The starting paper will all depend on how deep the dust is within the resin itself. If the dust is....
Tom (Staff)
-
7 Years Ago
Hi, I sand it with 600 grit then I end up with 1500 grit. Everything looks fine, but after I polish it with nw1 with a power tool, it became a bit hazy/Matt finish, not that glossy it was before. I a...
Nupur das gupta
-
7 Years Ago
If you can find aquabuff 1000 or 2000 it should be able to bring it back to a gloss finish
JasonFL
-
7 Years Ago
Good afternoon, Thank you for getting back in touch. It sounds as though a couple of things have gone wrong with the polishing process. If you are using a power tool with the NW1, you will need to.....
Tom (Staff)
-
7 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search